2507 Stainless Steel Coil
2507 Stainless Steel Coil
2507 stainless steel coil is a duplex stainless steel (EN 1.4410) with molybdenum and chromium contents of 4.0% and 25% respectively. It has been used in applications where the resistance to corrosion by weathering, seawater, and heat is required, as well as for food processing equipment and containers.
2507 stainless steel coil is readily welded by all methods except resistance welding. As a result of its good formability and weldability, these stainless steel coils material have been successfully used in heat exchanger tube, water treatment and water supply systems.
2507 Stainless Steel Coil Specifications
Product Name | 2507 stainless steel coil |
Grades | Duplex 2507/UNS S32750/EN 1.4410 |
Hardness | ≤30HRB |
Thickness | 0.02mm-6.0mm |
Width | 1.0mm-1500mm |
Edge | Slit/Mill |
Quantity Tolerance | ±10% |
Paper Core Internal Diameter | Ø500mm paper core, special internal diameter core and without paper core on customer request |
Surface Finish | NO.1/2B/2D/BA/HL/Brushed/6K/8K Mirror,etc |
Packaging | Wooden Pallet/Wooden Case |
Payment Terms | 30% TT deposit and 70% balance before shipment, 100% LC at sight |
Delivery Time | 5-7 working days |
MOQ | 200Kgs |
Shipping Port | Shanghai/Ningbo port |
Sample | The sample of 2507 stainless steel coil is available |
2507 Stainless Steel Coil Chemical Compositions
The chemical components of grade 2507 stainless steel coil is summarized in the following table:
Grade | Standard | C | Si | Mn | P | S | Cr | Ni | Mo |
2507 | ASTM A240 | ≤0.03 | ≤0.08 | ≤1.20 | ≤0.035 | ≤0.020 | 24.00-26.00 | 6.00-8.00 | 3-5 |
2507 Stainless Steel Coil Mechanical Properties
Grade | EN Grade | Yield Strength Rp0.2(N/mm²) | Tensile Strength Rm(N/mm²) | Hardness | Hardness(HB) | Elongation |
2507 | 1.4410 | ≥550 | ≥750 | Annealed | ≤310 | ≥20 |